CEM I 52,5 N Portland Cement
EN 197-1 Cement

CEM I 52,5 N Portland Cement

High-strength Portland cement for demanding structural work.

Description

A high-performance Portland cement engineered for demanding structural applications, providing superior 28-day compressive strength and excellent durability for critical infrastructure.

Application Areas
  • Long-span bridges and high-rise structural cores
  • High-strength precast and prestressed elements
  • Industrial and marine engineering projects
  • Specialty grouts and repair mortars
Sales Form / Packaging
  • 25–50 kg bags
  • 1.5 t sling bag
  • 1.5–2 t stretch hood
  • 1.5 t big bag
  • Bulk vessel / silo truck
Usage Conditions
  • Use within 90 days of production date for optimal performance.
  • Mix with potable water and clean aggregates conforming to EN 12620 / ASTM C33.
  • Do not use cement that has hardened or formed lumps.
Storage
  • Store in a dry, covered area protected from moisture and direct sunlight.
  • Stack bags on wooden pallets, no more than 10 bags high.
  • Rotate stock on a first-in, first-out basis.
Technical Specifications
Chemical Requirements
PropertyUnitStandard LimitTest Results
SiO₂%—18.70–21.60
Al₂O₃%—4.00–6.50
Fe₂O₃%—3.20–4.70
CaO%—61.70–66.60
MgO%—1.00–3.70
SO₃%Max 4.002.00–3.25
Cl%Max 0.100.0010–0.0400
Loss on Ignition (LOI)%Max 5.000.70–3.00
Insoluble Residue%Max 5.000.05–1.00
Free CaO%—0.30–3.00
Cr (VI)ppm—2–30
Na₂O%—0.02–0.32
K₂O%—0.30–1.10
Na₂O Eq.%—0.30–0.90
Lime Saturation Factor (LSF)–—96.00–105.30
Silica Modulus (SM)–—1.90–2.50
Alumina Modulus (AM)–—0.90–2.00
Physical & Mechanical Requirements
PropertyUnitStandard LimitTest Results
Specific Gravityg/cm³—3.11–3.21
Specific Surface (Blaine)cm²/g—3600–4500
Residue on 0.045 mm%—0.1–2.0
Residue on 0.090 mm%—0.0–1.0
Initial Setting TimeminMin 4590–220
Final Setting Timemin—130–320
SoundnessmmMax 10.00.0–4.0
Normal Consistency%—26.0–31.0
Compressive Strength (EN 196-1)
PropertyUnitStandard LimitTest Results
2 DaysMPaMin 20.024.0–35.5
28 DaysMPaMin 52.554.0–65.0